O.D. Cooling Water Corrosion in Slurry Bundle

chronicle companion images

IMAGE #1
Fixed Tube Sheet View of Straight Tube Bundle
Chron15-1.png
Recent failures which launched RCFA
IMAGE #2
Severe O.D. Corrosion – Cooling Water Corrosion
Chron15-2.JPG
O.D pitting of 65% depth
IMAGE #3
Multiple Pit Initiation Sites
Chron15-3.JPG
Note: Numerous initiation sites along tube axis
About & Subscribe
IMAGE #4
Chron15-4.jpg
IMAGE #5
Tube Support Location
Chron15-5.JPG
Corrosion cells adjacent to supports
IMAGE #6
Chron15-6.JPG
Thick/friable cooling water deposits on support structure